CuCrZr milteliai Cheminė sudėtis Element Weight % Copper Bal. Chromium 0.5 - 1.0 Zirconium 0.02 - 0.2 Iron <0.15 Silicon ≤0.10 Oxygen ≤0.10 Nitrogen ≤0.05 Mechaninės savybės Heat treatment Yield strength ≥420 MPa Tensile strength ≥520 MPa Elongation ≥20.0 % Electroconductibility ≥85.0 % Thermal conductivity Room temperature 100 ℃ ≥280 W/(mK) ≥300 W/(mK) Morfologija Particle size distribution D10 D50 D90 ≥15 µm 30 - 40 µm ≤60 µm Sphericity ≥0.9 Packing density ≥4.4 cm³ Packing density ≥5.2cm³ Flowability ≤22 s/50g +370 60062125+370 64028138 info@aamgroup.lt Užsisakyti!